1. Good electric conductivity and high thermal conductivity
2. Low thermal expansion and high resistance to thermal shock.
3. The strength increases at high temperature, and it can withstand over 3000 degrees.
4. Stable chemical property and hard to react
5. Self lubrication
6. Easy to process
1. Technical Index
Type | MSL80 | MSS80 | MSL85 | MSS85 |
Grain Size (μm) | 25 | 25 | 25 | 25 |
Bulk Density (≥g/cm3) | 1.8 | 1.8 | 1.85 | 1.85 |
Compressive Strength (≥MPa) | 60 | 60 | 70 | 70 |
Flexural Strength(≥MPa) | 30 | 30 | 35 | 35 |
Porosity(≤%) | 21 | 21 | 18 | 18 |
Specific Resistance(≤μΩm) | 12 | 12 | 12 | 12 |
Ash Content(≤%) | 0.08 | 0.08 | 0.08 | 0.08 |
Shore Hardness | 48 | 48 | 50 | 50 |
1) The ash content can be purified to 30ppm according to the requirement.
2) The above index data is the standard value, not the guaranteed value.
Graphite Products for Machined Tool
Graphite Products for Machined Tool
high strength Graphite Mould for powder sintering hard alloy